Product Overview
| Material | AISI 3130 steel |
| Heat-treatment Method | Quenched and Tempered |
| Suitable Application and Environment | Heavy Loading, Deep and Inhibited Corrosive Wells |
| Rod | Steel | Heat Treatment | Tensile Strength | Yield | Yield | Elongation | Reduction | Hardness | |
| ksi | Mpa | ksi | Mpa | 8″, % | % | RC | |||
| EHK | 3130 | Quenched & Tempered | 140/155 | 965/1068 | 130 min | 896 min | 11 min | 50 min | 30/35 |
| C | Mn | Mo | Cr | Ni | Cu | P | S | Si | V | Al |
| 0.22/0.29 | 0.71/1.00 | 0.05 max | 0.41/0.65 | 0.70/1.00 | 0.35 | 0.025 max | 0.035 max | 0.15/0.35 | – | – |